tendency to build up black needle-like whiskers - probably an effect of the high voltage present at sharp
edges (although the whiskers then cover the entire solder-covered surface of these plates) - see attached photo.
I‘m not sure yet what material they consist of - it looks like carbon to me but I should collect
some and give it to an analytical lab… could also be metal (tin from the solder pad?). In case it
is carbon, the usage of pure nitrogen gas (especially for VT gas) may help, but I don’t have any
hard data proving that.
As these build up over time they can lead to a higher tendency for arcing (certainly making the situation
worse and yet more whisker formation) and even create sort circuits between the coil windings, messing up
tuning & pulse width.
Unfortunately they can only be seen and cleaned up after removing the PFG coil (requiring soldering). The
photos show the little plate before and after cleaning.
Cheers
Bert
-> Sent via mobile <-
Spin-Doc
Magnetic resonance equipment, service, training & more
Dr. rer. nat. Bert Heise
Owner, applications scientist
Kiefernweg 13
58239 Schwerte
Germany
Mail:bert.heise_at_spin-doc.net
Phone: +49-171-5135315
Representing MestreLab software, Stelar relaxometers & BarthelHF amplifiers